| Sign In | Join Free | My entremaqueros.com |
|
| Categories | Inconel Alloy |
|---|---|
| Brand Name: | KAIXIN |
| Model Number: | KX-Alloy IN P718 |
| Certification: | ISO9001:2015 |
| Place of Origin: | China |
| MOQ: | 200KG |
| Price: | To negotiate |
| Payment Terms: | T/T, L/C |
| Supply Ability: | 50~80 TONS per MONTH |
| Delivery Time: | 45~60days |
| Packaging Details: | Wooden Box, size as per guests' request |
| Shape: | Wire,Strip,Rod,Pipe,Plate |
| Alloy Type: | Nickel-based Superalloy |
| Raw Materials: | NI Rem,CR18%,Co9% ,MO2.75% |
| Executive standard: | ASTM |
| Delivery State: | Soft State |
| Application: | Used for disc, brake, fastener, blade and etc |
| Features: | High temperature resistance |
| Size: | Negotiable |
| Company Info. |
| Danyang Kaixin Alloy Material Co., Ltd. |
| Verified Supplier |
| View Contact Details |
| Product List |
KX Inconel 718 Plus Nickel Alloy Wire Round Bar Tube Steel Sheet Light Rod On Inconel Alloy
Product Description and Application
Inconel718 plus is a new type of nickel-based precipitation-hardened alloy, which is widely concerned at home and abroad because of its excellent comprehensive mechanical properties below 700°C, good thermal working and welding properties, suitable cost. At present, this material has been promoted and applied in several well-known aero-engine companies, which are used in disc parts, brakes, fasteners, blades and etc. In addition, Inconel718 Plus is also commonly used in copper extrusion mold.
Process Performance and Requirements
Vacuum Induction Furnace(VIM) and Electroslag Remelting Furnace(ESR)
| Element | C | Ni | Cr | Mo | W | Co | Fe | Nb | Ti | Al | P | B |
| Inconel718 plus | 0.02 | Rem | 18 | 2.75 | 1 | 9 | 10 | 5.45 | 0.7 | 1.45 | 0.01 | 0.004 |
| Density | 8.25g/cm3 |
| Melting Temperature Range | 1260~1340℃ |
Hardness:
The hardness is about 20-30HRC after solid solution heat treatment and about 38-45HRC after annealing

Professional Customization
| Cold-drawn Wire | ¢0.3~¢18mm(Delivery in rolls or trays) |
| Hot-Rolling Wire | ¢5.5~¢20mm(Delivery in rolls) |
| Strip | thickness 0.1~4.5*width 6~350mm(Supply in rolls or straight strips) |
| Smooth Forged Rod on a Lathe | ¢60~350mm,L800-2500mm |
| Hot-rolled Burnishing | ¢20~80mm,L1000-5000mm |
| Cold Drawn and Burnishing | ¢2.5~18mm,L1000-8000mm |
| Seamless Tube | ¢1~275mm,wall thickness 0.2~30,L1000-8000mm |







|