OEM Hot Runner Typical Injection Molding Defects Analysis And Solutions

Categories Injection Molding Solution
MOQ: 100pcs
Price: Negotiable
Payment Terms: T/T
Supply Ability: More than 1 million
Delivery Time: 30day
Packaging Details: As the customer required
Place of Origin: CHINA
Brand Name: OEM
Certification: ISO
Emphasize: The Cause And Countermeasure Of Product Leaving Marks
  • Haven't found right suppliers
  • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
  • And this service is free of charge.
  • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
Submit Buying Request
  • Product Details
  • Company Profile

OEM Hot Runner Typical Injection Molding Defects Analysis And Solutions

The Cause And Countermeasure Of Product Leaving Marks

Current Ripple


When the material in the mold is solidified and the molten material after the flow is mixed, such as Mi is not fully integrated, there will be dim and scaly in the product. Iridescent or ring shaped, this phenomenon is the flow mark, usually occurs at a slow speed


CauseCuntermeasure
Forming condition

1. The material overflow degree is too low, and the front section is very easy to cure

2. Mold temperature is too low

3. The speed of chaos molding is too fast or too slow, which will produce ripple flow marks when it is too slow and jagged flow marks when it is too fast

4. The filling pressure or holding pressure is too low, so that the flow mark is clear

show

1. Increase the molding temperature

2. Increase die temperature

3. Set the right speed

4. Increase filling and retaining pressure


Die

1. The gate is too small

2. No cold feed well

3. Improper pouring U position


1.F pour n

2. Open more cold feed Wells.

3. If pouring U is not fixed, the material will also touch the position of trapping mold hole wall

Product Design

1. Product structure design makes more right angles

2. The product is broken and the thickness difference is too large

1. Improve product shape and smooth molten material flow

2. Change the design to make the thickness too smooth

Material

1. Poor liquidity of materials

2. Too much filler


1. Improve liquidity

2. Switch to materials with fewer fillers

OtherBlockage of suona on injection molding machine

Clean the nozzle of the machine


Quality OEM Hot Runner Typical Injection Molding Defects Analysis And Solutions for sale
Send your message to this supplier
 
*From:
*To: Sun On Plastic Moulding Limited
*Subject:
*Message:
Characters Remaining: (0/3000)
 
Inquiry Cart 0