| Sign In | Join Free | My entremaqueros.com |
|
| Categories | Turbine Blade Steel |
|---|---|
| Brand Name: | PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL |
| Model Number: | AMS 5674 |
| Certification: | SGS, TUV, BV, ISO, MTC |
| Place of Origin: | China |
| MOQ: | 800kg |
| Price: | Negotiations |
| Payment Terms: | T/T |
| Supply Ability: | 50000KGS/Month |
| Delivery Time: | Ex-stock for delivery: 3-7 days Production lead time: 30-60 days |
| Packaging Details: | Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement |
| Product Name: | AMS 5674 Superalloy Flat Bar |
| Characteristic: | Corrosion and Heat resisitant |
| Heat treatment condition: | +A, +AT, etc |
| Processing methods: | Peeld, Polished, etc |
| Available Shapes: | Forging piece, Tubing, Flat Bar |
| Surface: | Centreless Ground, Bright, etc |
AMS 5674 Superalloy Flat Bar
Product Information
AMS 5674 is a high-temperature alloy steel with excellent corrosion resistance and high-temperature performance. It is an alloy of molybdenum, cobalt, chromium, and nickel, commonly used for manufacturing parts that work under high temperature stress, such as blades in turbine engines and blades and rotors in gas turbines. AMS 5674 alloy has good mechanical properties and high-temperature stability, and can be used at temperatures up to 980 ° C. In addition, the alloy has excellent corrosion resistance and can resist corrosion and oxidation in extreme environments.
Size Range
Round bar / Wire rod (Diameter):1.0 mm to 1000 mm
Square bar / Flat bar: 1.0 mm to 1000 mm
Forging piece: Stepped shafts with flanks / discs /tubes /slugs
/donuts /cubes /other different shapes based on OEM.
Heavy/middle plate via hot rolled: T5.0 - 1000 mm X W3 - 1000 mm X
L100-1000 mm
Sheet steel via cold rolled: T1.0 - 10 mm X W1 - 1000 mm X L100 -
800 mm
Steel strip via cold rolled: T3.0 - 10 mm X W1.0 - 1000 mm X L (or
in coil form)
Length: Fixed length or random length or based on the customer's
special requirement.
Chemical Composition and standard
AMS 5674D | Mechanical Properties |
| SAE AMS 5674D | |
C(%): ≤0.08 Cr(%): 17.0~19.0 Ta(%): ≤0.05 Cu(%): ≤0.50 Fe: Remainder | Tensile strength,Rm/MPa: - Elongation, A/%: - Reduction of area, ψ/%: - Hardness HRC: - |

Applications
AMS 5674 is typically used to manufacture parts that operate under high temperature stress, such as blades in turbine engines and blades and rotors in gas turbines.
If you are interested in our products or have any questions, please
contact our team of engineers at
sales@ss-bars.com


|