| Sign In | Join Free | My entremaqueros.com |
|
| Categories | Metallographic Polishing Machine |
|---|---|
| Brand Name: | iqualitrol |
| Model Number: | XGrind-304 |
| MOQ: | 1 Set |
| Payment Terms: | T/T |
| Supply Ability: | 30 Sets per Month |
| Delivery Time: | 15 Working Days |
| Packaging Details: | Plywood Box |
| Application: | colleges and universities,scientific research institution |
| Diameter: | Disc Diameter φ203mm |
| Speed: | Rotation Speed 1400rpm |
| Power Supply: | AC220V/50HZ/1Ph |
| Motor: | 360W |
| Features: | steady running,small noise,convenient operation |
XGrind-304 Grinder Polisher Machine With Cabinet Double Plates CE Approved
Brief Introduction:
In the process of Metallographic sample preparation, polishing is a main procedure. After polishing on the machine,the sample surface is like a mirror. XGrind-304 Metallographic sample polishing machine is a classic polishing equipment with steady running,small noise,convenient operation and maintenance.
XGrind-304 meets the polishing requirement of all kinds of materials.This machine is suitable for factories and mines enterprises,colleges and universities,scientific research institution.
Technical Specifications:
| Model | XGrind-304 |
| Grinding/polishing disc diameter | φ203mm |
| Rotate speed | 1400r/min (900r/min alternative) |
| Input voltage | AC220V 50HZ |
| Disc quantity | 2 |
| Motor | 360W |
| Dimension | 570mm x910mm x1100mm |
| Net weight | 74kg |
Specimen Polishing:
Polishing discs are covered with soft cloth impregnated with abrasive diamond particles and an oily lubricant or water lubricant.
Particles of two different grades are used: a coarser polish - typically with diamond particles 6 microns in diameter which should remove the scratches produced from the finest grinding stage,
and a finer polish – typically with diamond particles 1 micron in diameter, to produce a smooth surface.
Before using a finer polishing wheel the specimen should be washed thoroughly with warm soapy water followed by alcohol to prevent contamination of the disc. The drying can be made quicker using a hot air drier.
Mechanical polishing will always leave a layer of disturbed material on the surface of the specimen. Electropolishing or chemical polishing can be used to remove this, leaving an undisturbed surface.
|