N-155 Superalloy, Multimet R30155 Cobalt Alloy Rod

Categories Precision alloy product
Place of Origin: Suzhou, China
Brand Name: AIWEN
Certification: SH
Model Number: SH-N-155
MOQ: 300kg
Price: Available per request
Packaging Details: By customers' require
Delivery Time: 25-30DAYS
Payment Terms: T/T
Supply Ability: 100000 KG per year
  • Haven't found right suppliers
  • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
  • And this service is free of charge.
  • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
Submit Buying Request
  • Product Details
  • Company Profile

N-155 Superalloy, Multimet R30155 Cobalt Alloy Rod

N-155 Superalloy, Multimet R30155 Cobalt Alloy Rod

Features of N-155 Superalloy, Multimet R30155 Cobalt Alloy Rod:

*N-155 alloy has high temperature properties which are inherent and do not depend upon age hardening
*It is recommended for applications involving high stresses at temperatures up to 1500°F, and can be used up to 2000°F where only moderate stresses are involved
*It has good ductility, excellent oxidation resistance, and can be readily fabricated and machined

Applications of N-155 Superalloy, Multimet R30155 Cobalt Alloy Rod:

It is commonly used for high-temperature bolts and aircraft parts, including:
*Tail pipes and cones
*Exhaust manifolds
*Nozzles
*Turbine, combustion chamber and afterburner components

Quality N-155 Superalloy, Multimet R30155 Cobalt Alloy Rod for sale